Time:[2015-6-3]  Hits:4732

Guangzhou Steel remind you: slab steel welding crack control measures
 

Guangzhou Steel slab steel member is large, plate thickness, weld deposit large, complex nodes, residual stress, prone to crack, affecting the quality of welding, which is important and difficult project quality control. Production of general measures are:
1, measures to prevent hot cracking
1) Control of the chemical composition of the weld. I.e. to reduce the low-melting eutectic composition readily segregation elements, such as sulfur and phosphorus content in the welding material and the base material is formed. Reduce the carbon content in the steel, can reduce the thermal cracking tendencies; improve Mn content can improve weld thermal cracking performance.
2) control of welding parameters and conditions. Control of welding current and welding speed, so that the aspect ratio of each cross section of the upper part of bead reach 1.1 to 1.2, can improve thermal cracking performance, while controlling the weld pool shape, do not form easily understood in sharp elongated bath a longitudinal weld surface thermal cracks. Preheat reduces tendency to form cracks; reasonable welding sequence can make the most of the weld at the smaller restraint of welding, reducing the tensile stress suffered weld shrinkage, thermal cracking tendency can be reduced.
2, cold cracking prevention measures
1) Before welding procedure qualification test performed to determine the process parameters.
2) preheat prevents cracking, as well as improve the performance of a certain action.
3) manual welding using low hydrogen electrodes alkaline E5Q / E55 type; CO: gas shielded arc welding flux cored wire can be used; a H08MnA submerged arc welding can be used F5021, and in strict accordance with the provisions drying. Drying temperature is 350-450 ℃, after dried at 100-150cC temperature for 1 ~ 2h, put insulation cylinder used with the check.
4) Choose a reasonable weld profile, in strict accordance with the drawings machining parts groove.
5) each side of the weld within the range of 30 ~ 50mm rust and water clean, reducing the source of hydrogen.
6) cracks often occur on the head welds and weld root, so tacking length, welding foot height and spacing should also make corresponding provisions. If you have to locate the weld in the groove proceeds, weld height should be less than 2/3 of the groove depth, the length should be greater than 40mm. If necessary, prior to tack welding is preheated. Before welding, positioning the weld inspection, it must be removed when re-welding cracks. Tack welding length and spacing, should be considered the base material thickness, structure length.
7) To reduce stress and prevent cracking during welding, the assembly should avoid forced assembly.
8) appropriate to increase the current, lower cooling rate, helps prevent the formation of hardened tissue.
9) Control interlayer temperature should be slightly higher preheat temperature.
10) Q345C soldering should be carried out after a slow cooling to slow cooling rate of the weld and heat affected zone and prevent cold cracking, respond promptly weldment insulation, that is immediately after welding weldment is heated to 250 to 350. And use of asbestos and other insulation 2.6h after air cooling can reduce the hydrogen content in the weld and prevent cold cracking, heating methods, with preheat before width.
Although Guangzhou Steel slab steel construction difficult, but as long as proper control measures, the proportion of component cracking will be greatly reduced, the project will significantly improve the quality of weld cracks will be avoided, can effectively control industrial building projects quality.

Copyright:佛山市胜邦钢结构有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粤ICP备13078463号
中国设备管理网>>设备管理网>>机电设备维修与管理网>>机电之家行业门户网| 生产型冻干机| 山东环保科技| 滚筒电子秤| 地下自卸车| 粉末硫酸铝| 市政工程管道| 山东临工配件批发价格| 超声波污泥界面仪| 空气放射性监测仪| 橡胶气囊| 智能候车亭| 地埋式生活污水净化槽定制厂家| 60HZ变频电源| FST镊子| 药品稳定性试验箱| 微库仑硫氯分析仪| SRY2管状电加热器| 钛材搅拌器| ATEX防爆风速仪| KIT便携式土壤水分仪| 环保石灰窑| 生化培养箱厂家| 化工粉尘处理器| 智能制造生产线| ZNCL智能磁力搅拌器| 引进型流量计| 液压油制动器厂家| 三防检修| 推流器桨叶| 刚性防水套管| 深圳市领航智造自动化| 鑫诚欣| Just加热器| 热轧移动剪切线厂家| 水雨情自动观测系统| 创力掘进机配件| 中国机械通用零部件工业协会| 锅炉气候补偿器| 氟化氢工业过程分析仪| KIESEL清管器|