Foshan Steel: steel structure fire retardant paint coating application methods Introduction

Time:[2015-1-17]  Hits:4864

Foshan Steel: steel structure fire retardant paint coating application methods Introduction

Different fireproof paint coating method is slightly different, but the basic coating process is similar. Below TN-LG fireproof coatings to illustrate the technical requirements of fireproof paint coatings.
TN-LG is a modified high temperature inorganic binder with expanded vermiculite, perlite and other heat-absorbing, heat insulation and fire protection coating material to enhance a chemical additives and synthetic materials.
(1) before painting steel components should be thoroughly rust treatment, it is best to brush the rust, so as not to appear and there will be a new rust before spraying fire retardant paint, should remove surface dust and dirt before spraying.
(2) coating the ambient temperature should be maintained at above 0 ℃, no drafts.
(3) the use of spray paint spraying equipment, each coating thickness of 5 ~ 10MM, separated by a 2 ~ 8H spraying until the required thickness so far, local repair manual wiping available.
(4) two-component coating, according to the ratio requirements before spraying the A, B two components deployed evenly. When deployed, the first dilute material into the mixer mixing 3 ~ 5MIN, then pour in the powder, such as 20 ~ 26KG mixing the material to the desired consistency can be sprayed.
Note: The painting should pay attention to this kind of two-component coating after mixing, paint curing faster, mixing time should be controlled within 10MIN, stirring after spraying within 20MIN, high summer temperatures should be faster.
(5) prepare cured and maintenance. Just spray the coating should avoid rain shower, room temperature coatings cured within 48 ~ 96H.
(6) paint stored at 4 ~ 40 ℃, not on the outside storage or exposure to the sun. Paint is valid for six months.

Copyright:佛山市胜邦钢结构有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粤ICP备13078463号
二手Sciex液质联用仪| 挥发物气体检测仪| 自动称重选别机| PVC电缆料造粒机| 青岛除甲醛| 逆反射标志测量仪| 智能型蓄电池参数测试仪| 电动扫地机厂家| 价格低| 真空袋| 进口食品级润滑油| 电缆直流耐压试验设备| 500T反力框架| 菲思图里氏硬度计| 电动百格试验机| 空调机组用安全阀| 果蝇监控| Dumont镊子| 无菌塑料拭子| 邳州聚氨酯保温管| 消防安装施工| 进口氮吹仪品牌参数| 平板离心机| InSb红外探测器| 环氧玻璃丝管| mdexx风机| 回收二手停车设备| JIENSI二甲苯气体检测仪| 广东金联宇厂家价格| 顶空气体分析仪| 自动化反应量热| 幼儿园设计| 平弹垫三组合| 特种电缆生产厂家| 酸雾废气吸收塔| 中频感应加热器| 机制砂生产线| 实验室双螺杆色母造粒机| SPR分子互作仪| 多元素火焰光度计| 角行程电动执行机构|